Fig.13-22 Corrosion of 304 SS exposed in flowing sodium for 82000 h

Fig.13-22 Corrosion of 304 SS exposed in flowing sodium for 82000 h

Corrosion due to dissolution of alloy elements in structural materials is observed in higher-temperature regions, and dissolved products are deposited in lower-temperature regions.