Fig.8-8 Change in the appearance of nuclear fuel material containing organic compounds subjected to heat treatment: (a) before heat treatment, (b) after heat treatment (200 ℃), and (c) after heat treatment (700 ℃)

The appearance of the nuclear fuel material changes from light brown to light green during heat treatment. After heat treatment, the volume decreases significantly as shown figure and the weight decreases by 70% from 104.34 g.